Float inside finished

Lamination of the Beamflange


I wetted out each BD layer on a sheet of plastic and put this "prepreg" in place.


Tempering the hull inside
To get the full strenght of the epoxy, i build a tent over the hulls and heated it up to 40 C. The temperature was keeped for 12h.


Prepearing the cutouts for the float deck


Float deck vakuum pressed


Second float ready for glueing the float deck.
On the float deck is the frame to lift the float deck single handed.


Float decked pressed on the float.
I used all heavy equipment to press the deck onto the float.